Ok mel, maybe this will help. Maybe not!

Crowell's Black
Albany or Alberta slip 170
om 4 ball clay 69
cobalt oxide 50
chrome oxide 25

Brush, spray, or pour this on as an underglaze. It's a very deep, dark
blue to black.