search  current discussion  categories  kilns & firing - gas 

help low pressure propane firing in low temp

updated tue 2 jan 01

 

Darlene Beverlin on sun 31 dec 00


I live in Missouri where is has not been above freezing since Nov 16th. =

I have a 60 cubic foot kiln with two burners. =20
The tank is 1000 gallon.
When the temp drops in the teens the pressure coming from the tank drops =
as well.
So low that I can not raise the temp and indeed the temp drops.

All of you that fire in the northern states must have some tricks up =
your sleeves. Please share them. I have to fire soon.=20

Thanks and have a sunshine day.

darlene
http://rarearth.tripod.com
rarearth@lyn.net