Jean Cochran on thu 21 dec 00
Plates Warping - Don't Listen To Me 2:
Dear Fellow Clay Arters,
Just finished setting out the rest of the plates (that I "wadded" 6 to 8
little wads and that were "spinners").
It seems that the plates that fired to cone 10 did not warp. The ones I
fired to cone 11 (the glazes want it that way), warped. All other
options remain the same as my previous post. However, I MAY not shoot
myself. It would make an ugly red stain in all this beautiful snow.
Jean Wadsworth Cochran
Fox Hollow Pottery
New Haven, KY
| |
|