search  current discussion  categories  materials - misc 

sv: re: glaze test for ron roy /dolomite violets

updated mon 25 dec 00

 

Alisa and Claus Clausen on sun 24 dec 00


Dear Ababy,
I use another dolomite white, posted as ToDo white which I am just about =
to make a career out of,=20
I like it very much. I painted on the surface with a mixture of cobalt, =
rutile and ball clay.=20
The lines in the drawing varied from dark blue to violet to green. =
Great looking changes in one painted line.
Best regards,
Alisa in Denmark