Carole Fox on wed 3 jan 01


Dear Deborah,
=20
You will need to reglaze and refire your piece. To get the glaze to =
stay on your piece, you will need to use something sticky such as a =
tacky hairspray or honey. It also helps to warm your pot before you =
reglaze it.=20

Now keep in mind; some glazes will run terribly on the second time =
around. You may want to take extra precautions to protect your kiln =
shelf. You may also choose not to reglaze all the way to the bottom of =
the pot.

Good luck!
Carole Fox-in Elkton, MD where the purple, pink and blue-gray clouds =
have melted from the sky, and my puppy and I wait for the sun to peek in =