search  current discussion  categories  technology - internet 

www.cantellostudios.com

updated mon 8 jan 01

 

Ababi Sharon on sun 7 jan 01


Plese let us know, when your site is ready! I keep in my comuter the picture
you have sent my of your Raku works (and recipe)
Ababi
----- Original Message -----
From: "Cantello Studios"
To:
Sent: Sunday, January 07, 2001 6:03 PM
Subject: Re: crystalline glazes


> Hi bill I to am interested in trying to grow crystals at cone 6. I have
been
> working at cone 10 for a long time and have had some good crystalline
growth
> but my kiln and my power are not in sink. The problem hears is my kiln
takes
> about 85 amps. And all I have coming into the studio is 100 amps. And the
> kiln is some 140ft. from the power source. I have the old power drain
thing
> going on but if I could work at cone 6 I may be able to pull this off. If
> you would be willing to share some glaze base starting points I would be
> very grateful. You could e-mail me off list at tleecan@2xtreme.net I thank
> you in advance. Chris soon to be at www.CantelloStudios.com my web site
will
> be up by the end of the month if not sooner.
>
> -----Original Message-----
> From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
> Behalf Of william schran
> Sent: Friday, January 05, 2001 2:08 PM
> To: CLAYART@LSV.CERAMICS.ORG
> Subject: Re: crystalline glazes
>
> Cheryl - I'd be happy to share whatever information I have. I've been
> working in crystalline glazes at cone 6 for a while and wrote an
> article for ClayTimes last Sept./Oct. issue. Please feel free to
> email me off line.
> Bill Schran
>
>
____________________________________________________________________________
> __
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.