tomsawyer on thu 11 jan 01


In Val Cushing's manual, he uses the term "atmospheric slip" Since I am =
awash in atmosphere, I have no idea what that means. Thanks for any =
replies.
Tom Sawyer
Orlando, Fl
tsawyer@cfl.rr.com

Dannon Rhudy on thu 11 jan 01


At 10:19 AM 01/11/2001 -0800, you wrote:
>In Val Cushing's manual, he uses the term "atmospheric slip" Since I am
awash in atmosphere, I have no idea what that means.....

Tom, he uses that to describe slips that will/may change color or
"flash" in atmospheric firings: wood firing, salt, gas. Not electric.

regards

Dannon Rhudy