Elizabeth Swenson on wed 31 jan 01


The May/June 1999 issues of Clay Times had a glaze recipe for a Hunter's
Green (it says it is from Corcoran School of Art and was furnished by
Grace Lewis). The recipe calls for Ferro Frit- but I don't know of a frit
called just Ferro Frit and neither does my regular supplier. I wrote to
Clay Times but haven't received an answer so am hoping someone knows
about this recipe and can help. What frit should I use?

Elizabeth Swenson
eswenson@mcn.org