Veena Raghavan on sat 27 jan 01
I wanted to let everyone who responded to me about Ron Roy's Black III and
my problems after my move, that I thinned the glaze and sieved it very
carefully. The test came out beautifully. So, it was just me! I think the
glaze had thickened, because it had been lying unused for a while, and the
container was probably not as airtight as it should be. I am so delighted,
as I really love this glaze.
Ron, my apologies for mistreating your beautiful glaze. Now, I am back on
track!
Thanks everyone.
Veena
Veena Raghavan
75124.2520@compuserve.com
| |
|