LOWELL BAKER on tue 30 jan 01
I have received a lot of requests for the plans for the sawdust
burner. The best published plans are in Nils Lou's Book "The Art of
Firing" I have changed the plans a little since I wrote that bit for
Nils. I will be happy to discuss the specifics of the change if you
are interested but take a look at the pictures in the book first. This
will help in our conversation.
Nils will certainly give me a cut in the new sales generated from
your interest.
Lowell
Nils Lou on wed 31 jan 01
right! Nils
On Tue, 30 Jan 2001, LOWELL BAKER wrote:
> I have received a lot of requests for the plans for the sawdust
> burner. The best published plans are in Nils Lou's Book "The Art of
> Firing" I have changed the plans a little since I wrote that bit for
> Nils. I will be happy to discuss the specifics of the change if you
> are interested but take a look at the pictures in the book first. This
> will help in our conversation.
>
> Nils will certainly give me a cut in the new sales generated from
> your interest.
>
> Lowell
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>
LOWELL BAKER on mon 4 feb 02
Many of you have asked for plans for my newest sawdust burner. I
will be providing these labelled photographs to those in attendance
at NCECA, but if you will not be there I can send you a copy. I will
have to charge there too because they don't pay for copying.
Send a SASE and two dollars or a mug, or anything else of
reasonable value to:
W. Lowell Baker
Department of Art
Box 870270
The University of Alabama
Tuscaloosa, AL
35487-0270
My apologies for asking for money, etc. I would rather have the
etc. Hope to see you at NCECA.
Lowell
Joseph Dallas on tue 5 feb 02
Hey Lowell,
Will you be at the Alabama Clay Conference? If so will you
have copies of the plans with you?
If so I'll trade ya a mug and a bottle of scotch for them.
See ya there,
Joe Dallas
Dallas Pottery & Architectural Ceramics
Columbus GA
jedallas@att.net
http://home.att.net/~jedallas
LOWELL BAKER wrote:
>
> Many of you have asked for plans for my newest sawdust burner. I
> will be providing these labelled photographs to those in attendance
> at NCECA, but if you will not be there I can send you a copy. I will
> have to charge there too because they don't pay for copying.
>
> Send a SASE and two dollars or a mug, or anything else of
> reasonable value to:
>
> W. Lowell Baker
> Department of Art
> Box 870270
> The University of Alabama
> Tuscaloosa, AL
> 35487-0270
>
> My apologies for asking for money, etc. I would rather have the
> etc.
| |
|