Snail Scott on tue 6 feb 01
At 11:38 AM 2/6/01 -0500, you wrote:
>What makes a glaze more durable?
>
>I have been looking at ceramic floor tiles and notice they are practically
all glazed in matt glazes, or at least have a matt surface.
>
>I was under the impression that a shiny glaze, one containing a lot of
silica, that is a high silica/alumina ratio was the most durable on
functional ware so why not for floor tiles too? Other than it being more
slippery, why the matt glaze or are ceramic floor tiles not really glazed
at all?
>
>Margaret Barlow
>Caistor Centre, Ont.
I think the non-slip factor is primary, but unlike
tableware, people don't often scrape pieces of
serrated steel across their floors on a daily basis.
Shoes are a lot kinder than knives, and most people
don't move their fridge daily. (If they did, their
floor would probably take similar damage, if the
little plastic knobs fell off the fridge feet.
Also, a matt surface may be easier to damage, but
it's harder to see the damage (and grime, and dust,
etc.) Polish scuff-marks off a shiny floor? No, thanx.
-Snail
Margaret Barlow on tue 6 feb 01
What makes a glaze more durable?
I have been looking at ceramic floor tiles and notice they are =
practically all glazed in matt glazes, or at least have a matt surface. =
I was under the impression that a shiny glaze, one containing a lot of =
silica, that is a high silica/alumina ratio was the most durable on =
functional ware so why not for floor tiles too? Other than it being =
more slippery, why the matt glaze or are ceramic floor tiles not really =
glazed at all?
Margaret Barlow
Caistor Centre, Ont.
Helen Bates on thu 8 feb 01
Hi,
I think that it's essential that any floor tile that may have water on
it (near street entrances of buildings, swimming pools, both decking
and change rooms, have non-slip surfaces. Whether this can be done
adequately with glazes I'm not sure. Perhaps a non-glazed highly
vitrified clay is what is used?
Helen
> ------------------------------
>
> Date: Tue, 6 Feb 2001 11:38:32 -0500
> From: Margaret Barlow
> Subject:
>
> What makes a glaze more durable?
>
> I have been looking at ceramic floor tiles and notice they are =
> practically all glazed in matt glazes, or at least have a matt surface. =
>
>
> I was under the impression that a shiny glaze, one containing a lot of =
> silica, that is a high silica/alumina ratio was the most durable on =
> functional ware so why not for floor tiles too? Other than it being =
> more slippery, why the matt glaze or are ceramic floor tiles not really =
> glazed at all?
>
> Margaret Barlow
> Caistor Centre, Ont.
>
> ---------------------
--
...........................
: Helen Bates :
: mailto:nell@quintenet.com :
...........................
| |
|