Alisa og Claus Clausen on sun 4 feb 01
Dear Annie,
Good for you, your officially here. Now the next learning module.
Look in the archives under mocha or moccaware (seen it both ways)
and you will find a wealth of practical inmformation. I did and I had =
mixed successes, but ultimately decided I did not like it as much as =
other decorative methods.
Intersting history and fun to make. The method I used called for a =
manganese wash over the white slip, so caution. I will be happy to tell =
you about how I made it, but I know there is at least one true mocha =
guru on the list. The only thing that comes to mind now is that I got =
really good branches when I used a very full brush of oxide right up on =
the edge of the painted slip, as opposed to painting in the middle of a =
slip ground. but there are many possibilities.
Best regards,
Alisa in Denmark
| |
|