Dear Alisa in Denmark- I'm so impressed that you took the time to write
this very detailed list of glaze-mixing instructions!

I have one little thing to add (since you asked ) and it is this:
Re-sieve each time I use each glaze. I began doing this years ago, when
I found that it is worth the time in smoothness of glaze application, as
sometimes tiny white crumbs seem to grow on their own in the glaze bucket,
(crystallization?) and if not removed, don't always melt during
firing!....very irritating!

Ann Brink in CA