search  current discussion  categories  glazes - specific colors 

blue green stoneware glaze and scrap glaze info

updated thu 22 feb 01

 

Mudnjoy@AOL.COM on wed 21 feb 01


In a message dated 2/21/01 9:24:46 AM US Mountain Standard Time,
drhudy@PARIS.CC.TX.US writes:

> I am looking for a blue green glaze for stoneware clay... nothing particular
> >in mind... i just want a nice glaze...
>
> Charlot,

Charlot and other blue green glaze seekers:
I get blue green glazes all the time with my "Scrap Glaze" process coming
up soon on my web site Artist's section soon. I mounted my test tiles last
night, my boyfriend promises to photo and scan while I'm on a business
trip/vacation. I'll provide the text as soon as I can. Are you wanting the
glaze for food containers?
I'll be at Art Camp for Grown Ups The Yuma Art Symposium this week. I'm
signing off for a while.
Joy In Tucson
URL: http://holdreadstudios.hypermart.net/
E-mail: Mudnjoy@aol.com
"Experience is what you get when you don't get what you want."