search  current discussion  categories  materials - misc 

chrome and tin oxides - no pinking occurred

updated thu 22 feb 01

 

Marianne Lombardo on wed 21 feb 01


Yesterday I opened the kiln and examined my work, and was pleased to see =
that the pot with chrome in it did not affect the other pots with tin =
oxide. I did keep them as far away as possible from each other, and =
kept the peepholes open and lid cracked for about 4 hours, so that may =
have helped.

Marianne Lombardo
Omemee, Ontario, Canada
email: mlombardo@nexicom.net