search  current discussion  categories  forms - misc 

flameware accidents?

updated thu 22 feb 01

 

David Jenkins on mon 19 feb 01




I am looking for information (first hand) on flameware accidents.  If you know of somebody who was either the potter or the victim I would like to get in touch with them.  or if you know of any articles in magazines I would like to be able to locate them.   Lili Krakowski mentioned that there may have been something in Clay Time so I have gone through all the back issues I have with no luck.  It is probably in the one issue I don't have.


Thank you     David Jenkins



Get your FREE download of MSN Explorer at http://explorer.msn.com



Lili Krakowski on wed 21 feb 01


I think it was in a Monona Rossol article. Maybe you could ask her?....

Lili Krakowski