search  current discussion  categories  materials - frits 

frit chart

updated sat 24 feb 01

 

Lyn Peelle on wed 21 feb 01


Does anyone out there know of a website or place I can get a list of Frits
and what they are made of? ie.--lead, etc?? And which are equivalent to
which??( Ferro/Pemb )
Thanks,
Lyn

Charles Moore on wed 21 feb 01


Lyn,

Check Frank Gaydo's web site. He had a pretty complete list of Frit
equivalents.

You might check the Laguna Clay website. Their catalog, pp. 78-81, contains
a good deal of information that should help you.

Charles
camoore33@earthlink.net
----- Original Message -----
From: "Lyn Peelle"
Subject: Frit Chart


> Does anyone out there know of a website or place I can get a list of Frits
> and what they are made of? ie.--lead, etc?? And which are equivalent to
> which??( Ferro/Pemb )
> Thanks,
> Lyn
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

Lawrence Ewing on thu 22 feb 01


Hi Lyn,

You can get some of this information at the Matrix website. Go straight to:

http://www.Matrix2000.co.nz/MatrialsWeb/default.htm

Lawrence Ewing

Senior Lecturer
Ceramics Department
School of Art
Otago Polytechnic
Dunedin
New Zealand

email: lewing@clear.net.nz

phone +64 03 472 8801

MATRIX GLAZE CALCULATION SOFTWARE:
http://www.Matrix2000.co.nz

GLAZETEACH:
http://www.Matrix2000.co.nz/GlazeTeach

MATRIX TUTORIALS:
http://www.Matrix2000.co.nz/MatrixTutorials

MATRIX ADDITIONAL MATERIALS RESOURCE:
http://www.Matrix2000.co.nz/MatrialsWeb/default.htm

-----Original Message-----
From: Ceramic Arts Discussion List [mailto:CLAYART@LSV.CERAMICS.ORG]On
Behalf Of Lyn Peelle
Sent: Thursday, February 22, 2001 8:06 AM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Frit Chart


Does anyone out there know of a website or place I can get a list of Frits
and what they are made of? ie.--lead, etc?? And which are equivalent to
which??( Ferro/Pemb )
Thanks,
Lyn

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Lili Krakowski on fri 23 feb 01


May 1978 William Hunt published a very complete list in Ceramics Monthly.
Many supplier catalogs have a frit chart for the frits they carry. I
expect the manufacturers will tell you if you write. If yu worry about
lead (and rightly so) or barium and lithium (and rightly so) ask your
supplier to tell you if yes/no there is that stuff in the frits they carr;
which/which not. As to web-sites: I need help to locate those
things...Can't help.

Lili Krakowski