search  current discussion  categories  techniques - stains 

iron & other stains

updated wed 28 feb 01

 

Des Howard on wed 28 feb 01


Fair go Mel!
My usual potting clothing is pretty much like the old surgeons
frock coats "covered in blood & laudable pus",
the white overalls are worn during the voluntary first aid work I do,
the stains come from hauling the muddy fallen from the
various arenas during rainy night Bacchanalia.
Des

I wrote:
Just bought it to see if it can remove red clay stains from my white overalls.

mel jacobson wrote:
iron stains. wear brown clothing. anyone knows that.
or, use porcelain, or burn the stain out. use a torch.

--
Des & Jan Howard
Lue Pottery
LUE NSW 2850
Australia
Ph/Fax 02 6373 6419
http://www.luepottery.lisp.com.au