search  current discussion  categories  glazes - cone 4-7 

^6 pink (mason stain reco)

updated thu 8 mar 01

 

cHuCk on wed 7 mar 01


Mason's Stain "Alpine Rose" holds pretty well at Cone 6.
We have used it for years. Needs a to have CaCo in the right amount to work
well.

Chuck



> Any cone 6 glaze which does not contain zinc should work with 6% addition
> of pink stain. However some pink stains are fugitive at this temperature.