search  current discussion  categories  glazes - misc 

sv: re: need a glaze..

updated sat 10 mar 01

 

Alisa og Claus Clausen on fri 9 mar 01


----- Original Message -----=20
From:
To:
Sent: Friday, March 09, 2001 2:58 PM
Subject: Re: need a glaze..
Dear Antonia,
The past couple of days with answers to cone 6 pink would most likely =
suit your stain. Raspberry Stain has these requiremnts, although it is =
glossy.
good luck,=20
Alisa in Denmark

.. This stain cannot have zinc in
> the formula and must have from 12 to 15% whiting. I need the help of =
some
> wonderful potter who can send me one or more glaze formulas. i fire =
at
> ^5-6-7 and i prefer glazes that are not too glossy!
>=20