search  current discussion  categories  glazes - traditional iron glazes 

hank's shino

updated thu 22 mar 01

 

Joyce Lee on tue 20 mar 01


Hank said:

> Should I imagine that I'm the Unnamed One with the KYSO shino? If so, I
> should tell you that I often glaze the other glaze first and the shino
> last, just to Break the Rule. So write me for Pat's Black Beauty to go
> under the shino.
> >
Yes, indeedy, you are he with the KYSO shino, Hank. Bet you didn't know
that I could be so closemouthed, did you? Not a word to a single soul
until now. Well, now, I can't wait to try layering shino on top of
another glaze .... one rule I faithfully adhered to .... should have
known better. Thanks for sharing that info. And I'll be writing within
minutes to find out about the black ... exciting! Thank you.

Joyce
In the Mojave