Christina Zola on thu 29 mar 01
An alternative to scooping (no need to figure out what to do with all that
rejected plaster of paris) -- don't fill the form all the way, and when it's
setting up, push a ball or some curved smaller form into the plaster to
hollow it out. Great for making very large molds... Keep it light!
| |
|