Dear Wallace,
this is Tony Hansens 5 x 20 glaze. Go to his great websit
Digitalfire.com and read about this base.
----- Original Message -----=20
From: wallace myers
To:
Sent: Sunday, April 01, 2001 6:44 PM
Subject: need a fix for crazing


Folks:

What would I do to the following glaze to correct crazing? I fire cone =
6 ox.

20.0 frit 3134
20.0 wollastonite
20.0 epk
20.0 flint
20.0 custer feldspar

Thanks.
Wallace

_________________________________________________________________________=
_____
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at =
melpots@pclink.com.

Alisa og Claus Clausen on sun 1 apr 01


Dear Wallace,
I just sent off a post too quickly, so if it hits the screen, here is =
the email finished.

The glaze you write is Tony Hansen's 5 x20, a base. I use it as it is =
with some whitener and do not experience crazing, but my clay, my =
materials, my kiln! Try another clay maybe, and be sure to read all =
about this glaze at Tony's great, fantastic, imformative website,
www.digitalfire.com
There you may find the solution after some testing.
Good luck,

Best regards,
Alisa in Denmark

Alisa Clausen
Varn=E6svej 171, DK6200 Aabenraa
Danmark
t. 45 7461 3641
Aliskin@mail.dk

Alisa's Pot Shop
Skolevej 3, DK6200, Aabenraa
Danmark
t. 20246640
Potshop@mail.dk