search  current discussion  categories  wheels - manufacturers 

a: brent wheel. any solutions?

updated sat 7 apr 01

 

Frank Gaydos on fri 6 apr 01


I agree with Jonathan.
We have 20 Brent wheels and abuse them every which way.
After 25 years they are still going and going like the bunny...
Seems the white plastic tuning fork shaped thingie in the foot
pedal gets brittle and lately have to replace them. Only had to
replace the control box speed controllers twice over the years.
If only my computer worked this well........
Good luck finding the problem.


----- Original Message ----- >
> These wheels are quite service free and built to last. Brent service has
> been incredibly helpful and very accommodating to me and have been quite
> cooperative in working with me over many years.

> Best
> Jonathan