I'm going to post some test glazes. They're all ^6 oxidation, and were fired
on brown stoneware clay, using a ramp program as follows. All temperatures
are listed in Fahrenheit.

300/hr to 2150
100/hr to 2200
Freefall to 1850
Hold for 1 hr
100/hr to 1750
Cooled naturally

Best wishes,

Cindy Strnad
Earthen Vessels Pottery
RR 1, Box 51
Custer, SD 57730
USA
earthenv@gwtc.net
http://www.earthenvesselssd.com

Michele D'Amico on mon 9 apr 01


Thanks for the glazes Cindy. It's kind of you to share. I'll try them and post my
results.
Michele D'Amico
Santa Cruz, CA

Cindy Strnad wrote:

> Dear Clayarters,
>
> I'm going to post some test glazes. They're all ^6 oxidation, and were fired
> on brown stoneware clay, using a ramp program as follows. All temperatures
> are listed in Fahrenheit.
>
> 300/hr to 2150
> 100/hr to 2200
> Freefall to 1850
> Hold for 1 hr
> 100/hr to 1750
> Cooled naturally
>
> Best wishes,
>
> Cindy Strnad
> Earthen Vessels Pottery
> RR 1, Box 51
> Custer, SD 57730
> USA
> earthenv@gwtc.net
> http://www.earthenvesselssd.com
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.