Jorna on tue 17 apr 01


r o n r o y kindly reworked jackies matt for my students but warns =
against using it as it has toxic amounts of lithia
i have not yet tested it(waiting for cadycal), anyway here it is,=20

Jackie's matt ^04
Frit 3134 - 32.0
CadyCal - 8.0
Talc - 5.0
Neph Sy - 6.0
EPK - 8.0
Silica - 35.0
Lithium Carb - 6.0 (toxic material)
Tin - 5.0
Total 105.0

Debbie Jorna

Ababi on tue 17 apr 01


How can I explain my students women that a glaze with lithium is poisonous?
Simply these glazes, I give them, just when the piece the way it is cannot
be used as a food container.I give them gloves.Not for all glazing only
Lithium , Barium and oxide washes. about this glaze,as a simbol, even if it
is not a soluble material. really beautiful, I cannot use as it is not gloss
and my students do not like unshiny surface.
Ababi Sharon
ababisha@shoval.ardom.co.il
http://members4.clubphoto.com/ababi306910/

----- Original Message -----
From: "Jorna"
To:
Sent: Tuesday, April 17, 2001 4:20 PM
Subject: jackie's matt ^04


r o n r o y kindly reworked jackies matt for my students but warns against
using it as it has toxic amounts of lithia
i have not yet tested it(waiting for cadycal), anyway here it is,

Jackie's matt ^04
Frit 3134 - 32.0
CadyCal - 8.0
Talc - 5.0
Neph Sy - 6.0
EPK - 8.0
Silica - 35.0
Lithium Carb - 6.0 (toxic material)
Tin - 5.0
Total 105.0

Debbie Jorna

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.