Vicki Conley on mon 16 apr 01
I tried using the Bailey glaze gun and tht ITC wouldn't go through. I hate
to just buy something else the wont't work. What should I use? Thanks
Vicki Conley
vicki@pinonpottery.com
www.pinonpottery.com
Ababi on tue 17 apr 01
I use EZE spray gun low cost and low clean.(takes seconds). You can buy some
bottles , so that you don't have to wash every second. If you have a big
amount of one type of glaze, you can add a narrow hose to make the original
longer and use from a different bottle, just remember to drill a tiny hole
in the cover of the bigger jar.
Ababi, in the land of milk and other stuff.
You can buy it from Big Ceramic Store As well as ClayartCenter.(just
remember not to save their E mail, otherwise they will get be default, all
the letters you send to Mel)!
Ababi Sharon
ababisha@shoval.ardom.co.il
http://members4.clubphoto.com/ababi306910/
----- Original Message -----
From: "Vicki Conley"
To:
Sent: Monday, April 16, 2001 5:36 PM
Subject: What kind of spray gun to spray ITC?
> I tried using the Bailey glaze gun and tht ITC wouldn't go through. I hate
> to just buy something else the wont't work. What should I use? Thanks
>
> Vicki Conley
> vicki@pinonpottery.com
> www.pinonpottery.com
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>
Lori Leary on tue 17 apr 01
Vicki,
Try a sandblaster gun, worked well for me.
Lori L.
Pawleys Island, SC
lleary@sccoast.net
| |
|