search  current discussion  categories  techniques - slips 

dry glaze?: desert slip

updated thu 3 may 01

 

Stephani Stephenson on tue 1 may 01


Not sure this fits the definition of a 'dry glaze' , but this is
wonderfully crusty yet durable, simple and useful
,wash/engobe/slip/glaze at cone 5-6.
Used it a lot on sculpture . easy to adapt.
Can't remember the source.

Desert Wash
borax 50
zircopax 50

Stephani Stephenson