cone 6 r

updated mon 29 may 06

 

Pancioli on fri 4 may 01


Thanks to June MacDonald for her generosity. She sent us many recipes
for cone 6R glazes. We will test them this summer and report to the
list.

Diana Pancioli

Diana Pancioli on fri 26 may 06


Hi All:

"Glazeforward", the cone 6 R glaze project I worked on this past year
is published in CM this month.

The website attached to the project is: glazeforward.com
where you can sign up to participate. The fee is $10.

This is a not for profit project, and monies collected
above expenses will be given to high school educators.

The article ends abruptly. There is more.
If you order the booklet you will get the whole thing.

Diana Pancioli
E.M.U.

Darnie Sizemore on sun 28 may 06


Pewabic Pottery has seen the glazes and they are
wonderful. Diana, I love this idea!!

Thanks,
Darnie

--- Diana Pancioli wrote:

> Hi All:
>
> "Glazeforward", the cone 6 R glaze project I worked
> on this past year
> is published in CM this month.
>
> The website attached to the project is:
> glazeforward.com
> where you can sign up to participate. The fee is
> $10.
>
> This is a not for profit project, and monies
> collected
> above expenses will be given to high school
> educators.
>
> The article ends abruptly. There is more.
> If you order the booklet you will get the whole
> thing.
>
> Diana Pancioli
> E.M.U.
>
>
______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change
> your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be
> reached at melpots@pclink.com.
>


__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com