Alisa og Claus Clausen on sat 5 may 01
Dear Lee,
Almost all of the =3DF3xides I use I blend with both rutile and Ball clay=
.. =3D
This gives a good painting consistency, and dampens the oxides' colors. =
=3D
I use roughly 1:3:5 ratio of oxide:rutile:ball clay. =3D20
I like to use cobal, iron and ochre, plus stains, where I would use =3D
double as much as an oxide.
Best regards,
Alisa in Denmark
| |
|