search  current discussion  categories  glazes - cone 8-10 

"wireless" ceramic stilts good to cone 10

updated fri 1 jun 01

 

Jim Kassebaum on thu 31 may 01


In response to several questions raised on 5/29/01, Laguna still offers
doubled pointed, all ceramic stilts. They work to cone 10 through numerous
firings unless used on a glazed surface in which case they normally have to
be replaced after each firing. See Laguna 1999/2001 Catalog p. 125.

Jim Kassebaum

Laguna Clay