search  current discussion  categories  kilns & firing - misc 

=?iso-8859-1?q?re:_kiln_sitters=ae?=

updated tue 22 may 01

 

Wade Blocker on mon 21 may 01


John,
The first thing I did to my Skutt cone 10 kiln, was to disconnect the
kiln sitter. I have always fired with cones and continue to do so. Mia in
ABQ