search  current discussion  categories  materials - misc 

french? plastic kaolin

updated thu 24 may 01

 

Ababi on sun 20 may 01


A supplier, here told me he could import French plastic kaolin called
DARVOR. Does anyone knows this kaoilin, is it plastic+ it's analysis?
He said it is used mainly for tiles.
Ababi Sharon
ababisha@shoval.ardom.co.il
http://members4.clubphoto.com/ababi306910/
http://www.milkywayceramics.com/cgallery/asharon.htm

Francoise Bazard on wed 23 may 01


Dear Abadi,
The "Kaolin d'Arvor" (ie. chinaclay) has the following composition :
K2O :1,1%
Al2O3 : 36,7 %
SiO2 : 48,5%
Lost at fire : 12,4 %
Impurities : 1,3 %
Have a good day
Sincerely
Fran=E7oise
--
Francoise Bazard
16, imp. de la Robertsau
67800 HOENHEIM (FRANCE)
mailto:francoise.bazard@beaux-arts.com
http://bazardceram.fr.st
http://www.multimania.com/fbazard