search  current discussion  categories  kilns & firing - coatings 

itc 100 shelf protection waning?

updated sun 20 may 01

 

C TRIPP on sat 19 may 01


Hi,
I would be interested to hear if anyone else has had the experience that Deb
describes below, when using ITC 100 as shelf protection. Anyone else find
that it became ineffective over time and what did you do? Spray on another
light coat?

I have my shelves sprayed but I only ever have small drips that chip off
easily or BIG melts that need a bag around the shelf and a hammer to smash
them off. (Oddly enough, it is only when I use the chemicals I bought off a
retiring potter who is now a dog groomer do I have big accidents. Makes you
wonder...voodoo epk!)

Best regards,
Carol
It's so hot here that I put some wet test "mice" out in the sun this morning
and they were bone dry in three hours and hot to the touch.


On Fri, 18 May 2001 10:14:53 -0700, Ceramic Arts Discussion List, Deb
wrote:

> I had ITC put on my shelves , walls, and elements (airbrushed on) when I
> got my new kiln a few years ago. For a while the ITC acted just like
kiln> wash (bits of glaze popped right off), but after a dozen or so
firings, the> protection waned.