search  current discussion  categories  materials - kiln wash 

kiln wash for salt

updated thu 24 may 01

 

Farrero, Charley on tue 22 may 01


Before the existence of ITC .....what was the formula for kiln wash for
spraying the walls of a new salt kiln
Ratio alumina / Kaolin ?
any of the pre ITC crowd remember?
thanks
Charley Farrero
farrero@siast.sk.ca
Ceramics dept. WOODLAND CAMPUS
BOX 3003- PRINCE ALBERT.SK.
S6V 6G1 CANADA
ph:(306) 9537064 fax:(306) 9537099
http://www.siast.sk.ca/~woodland/dos/community/ceramic/
studio: Box 145 Meacham S0K 2V0 306-3762221
cfjj@sk.sympatico.ca
http://www.saskterra.sk.ca/profile.htm
http://www3.sk.sympatico.ca/handwave/hcharley.html

Marcia Selsor on wed 23 may 01


50 Alumina and 50 kaolin
Marcia in Montana
leaving today for Italy workshop, signing off clayart. Ciao!

"Farrero, Charley" wrote:
>
> Before the existence of ITC .....what was the formula for kiln wash for
> spraying the walls of a new salt kiln
> Ratio alumina / Kaolin ?
> any of the pre ITC crowd remember?
> thanks
> Charley Farrero
> farrero@siast.sk.ca
> Ceramics dept. WOODLAND CAMPUS
> BOX 3003- PRINCE ALBERT.SK.
> S6V 6G1 CANADA
> ph:(306) 9537064 fax:(306) 9537099
> http://www.siast.sk.ca/~woodland/dos/community/ceramic/
> studio: Box 145 Meacham S0K 2V0 306-3762221
> cfjj@sk.sympatico.ca
> http://www.saskterra.sk.ca/profile.htm
> http://www3.sk.sympatico.ca/handwave/hcharley.html
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

--
Marcia Selsor
selsor@imt.net
http://www.imt.net/~mjbmls
http://www.imt.net/~mjbmls/Tuscany2001.html