search  current discussion  categories  materials - frits 

new frit

updated sat 19 may 01

 

will edwards on thu 17 may 01


Hello,

I have the information for Frit 439 should anyone be looking for it now. =
Its
another GB replacement source but available through a large company which=

means if you like it, it should be easy to get when needed.
Currently Daven's in Atlanta stocks it.

William Edwards

____________________________________________________________________
Get free email and a permanent address at http://www.netaddress.com/?N=3D=
1

william schran on fri 18 may 01


Folks- I'm going to be using Dal Tile frit #439 as the base for all
our class raku glazes this semester. I'm starting with a base of:
#439 - 80%, EPK - 20%. Melts well at cone 08 (and below), clear
gloss, crackles well based on a few fast fire tests in a small test
kiln. Will let you know how the results are later this summer.
Bill

scott lykens on fri 18 may 01


Deluxe, please tell us more, perhaps::

which large company makes it?
If it is not distributed by who makes it, which large company distributes
it?

Hows it work, most frit companies will be glad to post the percentage of
whats in a frit, does this one??

work better than cc 298??

just curious, thanks>
>
>Hello,
>
>I have the information for Frit 439 should anyone be looking for it now.
>Its
>another GB replacement source but available through a large company which
>means if you like it, it should be easy to get when needed.
>Currently Daven's in Atlanta stocks it.
>
>William Edwards
>
>____________________________________________________________________
>Get free email and a permanent address at http://www.netaddress.com/?N=1
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com