search  current discussion  categories  kilns & firing - manufacturers 

old paragon kiln working!

updated sun 20 may 01

 

Deb Erikson on sat 19 may 01


Thanks to all! =20
It turned out to be the kiln-sitter connections. My mood has improved =
ENORMOUSLY! Actually I haven't cleaned the connections yet, just =
switched it to manual and I got POWER! (ha - might try reading the =
manual next time....) My husband is jubilant since I thought the problem =
was his wiring... Now I'll make sure all the elements are working and =
test the temp, but it looked good!
THANKS AGAIN!
Deb in OK