repairing hair line cracks

updated thu 31 may 01

 

Ron & Nancy on tue 29 may 01


Beth,
Try the mixture of 1/3 your clay body slip, 1/3 vinegar and 1/3 karo
syrup. Paint it in to crack until it's solid again. let it settle and
dry, then glaze and fire. Should work, works for me.
Nancy