search  current discussion  categories  materials - misc 

sub for lepidolite

updated fri 1 jun 01

 

Nick Parker on wed 30 may 01


I was just wondering if anyone knows any substitutes for lepidolite. I
need if for a Crater glaze. So I need the gases it produces. Or if anyone
has any glaze recipes for crater glazes.
thanks
nick

Hank Murrow on wed 30 may 01


>I was just wondering if anyone knows any substitutes for lepidolite. I
>need if for a Crater glaze. So I need the gases it produces. Or if anyone
>has any glaze recipes for crater glazes.
>thanks
>nick

Dear Nick;

Try using spodumene and a small addition of Cryolite.

Hank

Ababi on thu 31 may 01


Please send the recipe and I see what I can do.
Please enter to my site, and tell me if you like my "Craterism"
Ababi Sharon
ababisha@shoval.ardom.co.il
http://members4.clubphoto.com/ababi306910/

----- Original Message -----
From: "Nick Parker"
To:
Sent: Thursday, May 31, 2001 4:44 AM
Subject: Sub for Lepidolite


> I was just wondering if anyone knows any substitutes for lepidolite. I
> need if for a Crater glaze. So I need the gases it produces. Or if
anyone
> has any glaze recipes for crater glazes.
> thanks
> nick
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>