Hi Yall,
Does anyone have a claybody recipe using Newman red for mid to high fire
temperatures ?
Thanks,
Merrie

Wesley C. Rolley on mon 18 jun 01


> Does anyone have a claybody recipe using Newman red for mid to high fire
>temperatures ?
>Thanks,
>Merrie
Merie,

The Claymaker in San Jose, CA has a ^10 stoneware that they call Cinnamon.
If I remember correctly this contains a significant (30+%) amount of Newman
Red. http://www.claymaker.com gives you their contact info. The owner,
Bob, has been very helpful to me.