search  current discussion  categories  materials - frits 

mason frit 6908; general color gf 136;

updated thu 21 jun 01

 

Helen Bates on wed 20 jun 01


Dear Ron Roy,

Re: Mason Frit 6908:
Through Northern Light's search engine I found this url, from which I
quote below:

http://www.marjonceramics.com/pages/products.html#MASON
Scroll down to "FRITS, STAINS AND GLAZES" then click on: STAIN DESCRIPTION>
Scroll down to find the section quoted below.

As you can see, there is a flux listed with the number "6908".
Perhaps this is what you are looking for.
Not much to go on, but the elements at least are listed.

>
> White-Flux See
> # Extender Al B Ca Pb Si Sn Zr Ref.
> 6700 White X X X 3,6
> 6768 Tin White X X X 3,6
> =======> 6908 Flux X X X 2 <========
> 6910 Flux X X X 2
> 6942 Flux X X X X X 2
> 6950 Flux X X X 2
> 6983 Flux X X X 2



Re: General Color GF-136:
General color GF 136 is listed for comparison to other frits at the
following url:
http://www.bigceramicstore.com/Information/frit_comparisons.htm

I include the relevant section of the comparison chart here:

==================================================================================
> LEAD-FREE FRIT EQUIVALENTS
>
> FERRO GENERAL PEMCO MOBAY FUSION OHOMMEL
> BAYER
>
> 3819 GF-136

==================================================================================

I hope to have been of some help.

Your neighbour in
Belleville.

Helen
--

===========================
Helen Bates
mailto:nell@quintenet.com
===========================