Ron Collins on sat 23 jun 01
The other day, someone was asking about the Greek method of black and =
red, --it's explained on page 39 of Karin Hessenberg's Sawdust =
Firing--part of the Complete Potter series. I don't know if you will =
get a more detailed step by step, I think there will be alot of trial =
and error....Melinda in Guatemala
| |
|