Cat Jarosz on wed 27 jun 01


Hi just a thought but you can flip shelves from front to back or another
way to say that is if this firing you had 2 posts in front and one in the
back next firing reverse that.... Its what I do but I do flip top to
bottom on the plate setters, learned the hard way on that but then again no
kiln wash on plate setters.... Cat.... who wishes she could see her bob
white family like Joyce in mojave can but enjoys listening to them sing
to her.... and trying to get her basset hound to chase the squirrels that
moved in away from the bird feeders LOL .... ya wanna talk futile !!!