Larry Zimmerman on wed 4 jul 01
Strontium Chloride is what I've heard will produce interesting luster
effects, but that's all I know.
How can you obtain luster iffects in an electric kiln using strontium
chloride?
What is the process - temperature - firing duration?
Any info would be greatly appreciated.