Hannah on thu 12 jul 01
Thanks to Ron Roy and Debbie Grant for noticiing I left an ingredient =
out of the buttermilk recipe. What is missing is 6.8 dolomite. Here =
it is again, and my apologies. It is a very nice waxy glaze.
BUTTERMILK ^9-10 Oxidation or Reduction
Custer Feldspar 29.3
Flint 24.1
Talc 13.5
Gerstley Borate 10.5
Whiting 9.0
Dolomite 6.8
EPK 6.8
100%
Zircopax 8%
| |
|