Duane Archer on thu 19 jul 01


How lucky can you get----I allowed my pot and large fish like fins
to completely dry before attaching with slip. They never cracked or fell off
and did not warp during the final glaze firing. My problems are the same as
you'all, so I tried what I knew would not work.----- Again--How lucky can I
get?????? Duane Archer in hot, humid and dry Oklahoma.