Jeff Osborne on wed 18 jul 01


kathleen L&L makes a really nice piece of equipment, both functionally and
artistically. However with the lid
movin' the way it is, the kiln will under fire maybe one cone, just because
of amount of heat loss. they are working on
the problem right now and think they have a solution to the problem but
want to test fire there kilns before sending it to
me. I am very happy with the kiln itself. the element holders are a great
idea.. I opted for heavy duty elements, industrial thermocouples, 3" brick,
vent and the hinged lid. I will be using the kiln strictly in tile
production so I needed all that and
then some.

gotta go

Jeff Osborne
Osborne Designs
Handmade tile Co.