John Forstall on thu 19 jul 01
The following glaze works beautiful at cone 6 for dipping, but when sprayed
it beads up and dusts off easily when dry. All my other glazes spray a nice
smooth wet surface. Adding water helps but then it curtains and runs off
the bisque. Increasing spray pressure don't help. Bisque is fired to large
cone 04. Question is which components could be culprit? Has anyone had
problem like this? Thanks for any replies.
Dolomite 15
Neph Syen 15
EPK 12
Ball Clay 08
Flint 21
3134 19
Lithium Carb 03
PVC 07
Titanium 05
John