search  current discussion  categories  kilns & firing - gas 

propane bottle size solved

updated sun 29 jul 01

 

Jim Tabor on sat 28 jul 01


Thanks to all responding to my post on propane. I bought 2 - 30# tanks, jointed with a special T to
allow gas to flow only one way. I have fired 8 loads (atmospheric burner) on less than 8# of gas. Works
great and is portable enough to easily move between home, school, and the lake. Not the slightest chill
on the tanks.