search  current discussion  categories  glazes - crazing & crackle 

: cone 6 crackle/dropping dead

updated fri 3 aug 01

 

iandol on thu 2 aug 01


Just out of curiosity I was looking at some imported soup bowls on the =
shelves in Woolies the other day. Nice form, good weight, adequate =
capacity and pleasing decoration. Sgrafitoed blue slip and a clear =
glaze. A very clear, very crazed glaze!!!

So if there are problems in the future with thes, where does the "Buck =
stop"?

Best regards,